Effect of adding clay on the rheological properties of the samples before/after aging and after re-homogenization.

Samples Before aging
After aging
After re-homogenization
Gel Strength (%) Gel 10 s Gel 10 min Gel 10 s Gel 10 min Gel 10 s Gel 10 min
2 wt.% H20 + 2 wt.% ORS VIS 100 100 81.9 100 97.3 100
5 wt.% H17 + 2 wt.% ORS VIS 100 100 90 100 98.5 100
5 wt.% R104 + 2 wt.% ORS VIS 100 100 89.1 100 100 100